Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 72.4 MPa
10500 psi
ASTM D638
Flexural Strength 114 MPa
16500 psi
ASTM D790
Flexural Modulus 3.79 GPa
550 ksi
ASTM D790
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 143 °C
290 °F
ASTM D648