Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 1100V-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100V-10 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0035 cm/cm | 0.0020 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 1200-10 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2103-20 CR-SX Fiberglass Reinforced Thermoset BMC Premi-Glas® 2103-20 CR-SX is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regu.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2200-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2200-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2200-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Pigmentable for molded-in c.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2200-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2203-22 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-22 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2203-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2203-25 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-25 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2205-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2205-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2205-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 3200-30 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-30 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH GF8030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2103-10 CRSX Polyester BMC Premi-Glas® 2103-10 CR-SX is a 10% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH GF4030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH GF8030 PB Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH GF8030 PD1 VT2 PP, Glass Fiber-Reinforced, Chemically Coupled Heat Stabilized Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | ASTM D955 |
PolyOne Edgetek® AS-10CF/000 FR Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued Description/Features:Carbon Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0035 cm/cm | 0.0030 - 0.0035 in/in | Compression Molding; ASTM D955 |
Sumitomo Bakelite North America E 8354-19189-2 Electrical Encapsulation Grade Epoxy Glass and mineral reinforced epoxy molding compound, formulated for the encapsulation of devices requiring high quality and thermal shock resistance.Information provided by Vyncolit, a Sumitomo Bak .. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0035 cm/cm | 0.0020 - 0.0035 in/in | |
Bulk Molding Compounds BMC 615 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 615 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ext.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | |
Bulk Molding Compounds BMC 851 Corrosion Resistant, Flame Retardant Molding Compound BMC 851is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications ar.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH GF5035 PD2 VT Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled/Heat Resistant Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Compression Molding. ASTM D955 |
Sumitomo Bakelite North America FS-80-P-1 Long-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GI.. |