Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
Polimeri Europa Extir® CM Galileo Europa 5 AE Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
Polimeri Europa Extir® CM Galileo Europa 5 Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
Polimeri Europa Extir® LN 5000 Expandable Polystyrene Extir LN 5000 belongs to the product family, the Leonardo Series, with these features: high expandability, high moulding productivity, wide processing area, optimal fusion and mechanical strength, e.. |
|||
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
Polimeri Europa Extir® Verdi VR A5000 AE Expandable Polystyrene - Flame Retardant b>Product Description:Extir Verdi VR A5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does.. |
|||
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
Polimeri Europa Extir® CM Galileo Io 5 AE Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
Polimeri Europa Extir® CM Galileo Io 5 Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
Polimeri Europa Extir® CM Giotto 5 AE Expandable Polystyrene - Continuous Mass/Flame Retardant Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
Polimeri Europa Extir® CM Giotto 5 Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
Polimeri Europa Extir Leonardo A 5000 AE Expandable Polystyrene
(discontinued **) Extir A 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext.. |
|||
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
Polimeri Europa Extir Leonardo B 5000 AE Expandable Polystyrene
(discontinued **) Extir B 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext.. |
|||
Particle Size | 900 - 1400 µm | 900 - 1400 µm | |
Polimeri Europa Extir® D 5000 AE Expandable Polystyrene
(discontinued **) Extir D 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext.. |
|||
Particle Size | 900 - 1250 µm | 900 - 1250 µm | |
SYNTHOS Koplen® 0814 F Expandable Polystyrene Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to moldings and block.Specific Characteristics: Flammability .. |
|||
Particle Size | 900 - 1250 µm | 900 - 1250 µm | |
SYNTHOS Koplen® 0814 FR Expandable Polystyrene Low Pentane Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to molded bricks and blocks. Lower density can be.. |
|||
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
SYNTHOS Koplen® 0822 FR Expandable Polystyrene Low Pentane Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to molded bricks and blocks. Lower density can be.. |
|||
Particle Size | >= 900 µm | >= 900 µm | |
Shandong Dongyue Polymer DF-21C PTFE Presintered Resin Usage: The presintered resin is suitable for continuously extruding of all types, pushing and pressing PTFE rod, tube and special shape.Packing: PTFE is packed in double layer PVC bags inside and in.. |
|||
Particle Size | 900 µm | 900 µm | <2% |
Shandong Rike Chemical HELIâ„¢ HLC-135A PVC Impact Modifier-CPE Series Mechanism of Impact ModificationIt is found by research that the weak impact strength of PVC under lower temperature is mainly caused by stronger intermolecular force of PVC. Owing to stronger inte.. |
|||
Particle Size | 900 µm | 900 µm | <2% |
Shandong Rike Chemical HELIâ„¢ HLC-2235 PVC Impact Modifier-CPE Series Mechanism of Impact ModificationIt is found by research that the weak impact strength of PVC under lower temperature is mainly caused by stronger intermolecular force of PVC. Owing to stronger inte.. |
|||
Particle Size | 900 µm | 900 µm | <2% |
Shandong Rike Chemical HELIâ„¢ HLC-3235 PVC Impact Modifier-CPE Series Mechanism of Impact ModificationIt is found by research that the weak impact strength of PVC under lower temperature is mainly caused by stronger intermolecular force of PVC. Owing to stronger inte.. |
|||
Particle Size | 900 µm | 900 µm | <2% |
Shandong Rike Chemical HELIâ„¢ HLC-40B PVC Impact Modifier-CPE Series Mechanism of Impact ModificationIt is found by research that the weak impact strength of PVC under lower temperature is mainly caused by stronger intermolecular force of PVC. Owing to stronger inte.. |
|||
Particle Size | 900 - 1400 µm | 900 - 1400 µm | |
Polimeri Europa Extir® D 5000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir D 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does not conta.. |