Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
Polimeri Europa Extir® CM Galileo Europa 5 AE Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
Polimeri Europa Extir® CM Galileo Europa 5 Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
Polimeri Europa Extir® LN 5000 Expandable Polystyrene Extir LN 5000 belongs to the product family, the Leonardo Series, with these features: high expandability, high moulding productivity, wide processing area, optimal fusion and mechanical strength, e.. |
|||
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
Polimeri Europa Extir® Verdi VR A5000 AE Expandable Polystyrene - Flame Retardant b>Product Description:Extir Verdi VR A5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does.. |
|||
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
Polimeri Europa Extir® CM Galileo Io 5 AE Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
Polimeri Europa Extir® CM Galileo Io 5 Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
Polimeri Europa Extir® CM Giotto 5 AE Expandable Polystyrene - Continuous Mass/Flame Retardant Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
Polimeri Europa Extir® CM Giotto 5 Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
Polimeri Europa Extir Leonardo A 5000 AE Expandable Polystyrene
(discontinued **) Extir A 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext.. |
|||
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
Polimeri Europa Extir Leonardo B 5000 AE Expandable Polystyrene
(discontinued **) Extir B 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext.. |
|||
Particle Size | 900 - 1600 µm | 900 - 1600 µm | |
SYNTHOS Koplen® 0822 FR Expandable Polystyrene Low Pentane Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to molded bricks and blocks. Lower density can be.. |
|||
Particle Size | 1250 - 1600 µm | 1250 - 1600 µm | |
SYNTHOS Koplen® 1020 F Expandable Polystyrene Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to blocks.Specific Characteristics: Flammability according to.. |
|||
Particle Size | 1250 - 1600 µm | 1250 - 1600 µm | |
SYNTHOS Koplen® 1020 FR Expandable Polystyrene Low Pentane Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into thick walled products and blocks. Lower density can be ach.. |