Polimeri Europa Extir® CM Giotto 5 AE Expandable Polystyrene - Continuous Mass/Flame Retardant

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Extir®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Extir® CM Giotto 5 AE Expandable Polystyrene - Continuous Mass/Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of blowing agent. Extir CM does not contain CFC or HCFC. Extir CM Giotto 5 AE is a white product with improved thermal conductivity.Applications: Extir CM Giotto 5 AE has an improved coefficient of thermal insulation. It is used mainly in the construction sector where, for legislative or safety reasons, the used of flame retardant material is required. Typical applications are: blocks for general purpose insulationexternal thermal insulation boards with improved lambdaInformation provided by Polimeri Europa.
Physical Properties Metric English Comments
Bulk Density 0.590 - 0.630 g/cc
0.0213 - 0.0228 lb/in³
Density >= 0.0100 g/cc
>= 0.000361 lb/in³
Minimum apparent density on a continuous pre-expander after two expansions
>= 0.0130 g/cc
>= 0.000470 lb/in³
Minimum apparent density on a discontinuous pre-expander
>= 0.0150 g/cc
>= 0.000542 lb/in³
Minimum apparent density on a continuous pre-expander after one expansion
0.0110 - 0.0200 g/cc
0.000397 - 0.000723 lb/in³
Density range normally used
Particle Size 900 - 1600 µm
900 - 1600 µm