Physical Properties Metric English Comments
Particle Size 900 - 1600 µm
900 - 1600 µm
Polimeri Europa Extir® CM Galileo Europa 5 AE Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
Particle Size 900 - 1600 µm
900 - 1600 µm
Polimeri Europa Extir® CM Galileo Europa 5 Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
Particle Size 900 - 1600 µm
900 - 1600 µm
Polimeri Europa Extir® LN 5000 Expandable Polystyrene
Extir LN 5000 belongs to the product family, the Leonardo Series, with these features: high expandability, high moulding productivity, wide processing area, optimal fusion and mechanical strength, e..
Particle Size 900 - 1600 µm
900 - 1600 µm
Polimeri Europa Extir® Verdi VR A5000 AE Expandable Polystyrene - Flame Retardant
b>Product Description:Extir Verdi VR A5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does..
Particle Size 900 - 1600 µm
900 - 1600 µm
Polimeri Europa Extir® CM Galileo Io 5 AE Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
Particle Size 900 - 1600 µm
900 - 1600 µm
Polimeri Europa Extir® CM Galileo Io 5 Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
Particle Size 900 - 1600 µm
900 - 1600 µm
Polimeri Europa Extir® CM Giotto 5 AE Expandable Polystyrene - Continuous Mass/Flame Retardant
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
Particle Size 900 - 1600 µm
900 - 1600 µm
Polimeri Europa Extir® CM Giotto 5 Expandable Polystyrene - Continuous Mass
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of ..
Particle Size 900 - 1600 µm
900 - 1600 µm
Polimeri Europa Extir Leonardo A 5000 AE Expandable Polystyrene  (discontinued **)
Extir A 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext..
Particle Size 900 - 1600 µm
900 - 1600 µm
Polimeri Europa Extir Leonardo B 5000 AE Expandable Polystyrene  (discontinued **)
Extir B 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext..
Particle Size 900 - 1400 µm
900 - 1400 µm
Polimeri Europa Extir® D 5000 AE Expandable Polystyrene  (discontinued **)
Extir D 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext..
Particle Size 900 - 1250 µm
900 - 1250 µm
SYNTHOS Koplen® 0814 F Expandable Polystyrene
Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to moldings and block.Specific Characteristics: Flammability ..
Particle Size 900 - 1250 µm
900 - 1250 µm
SYNTHOS Koplen® 0814 FR Expandable Polystyrene
Low Pentane Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to molded bricks and blocks. Lower density can be..
Particle Size 900 - 1600 µm
900 - 1600 µm
SYNTHOS Koplen® 0822 FR Expandable Polystyrene
Low Pentane Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to molded bricks and blocks. Lower density can be..
Particle Size >= 900 µm
>= 900 µm
Shandong Dongyue Polymer DF-21C PTFE Presintered Resin
Usage: The presintered resin is suitable for continuously extruding of all types, pushing and pressing PTFE rod, tube and special shape.Packing: PTFE is packed in double layer PVC bags inside and in..
Particle Size 900 µm
900 µm
<2%
Shandong Rike Chemical HELIâ„¢ HLC-135A PVC Impact Modifier-CPE Series
Mechanism of Impact ModificationIt is found by research that the weak impact strength of PVC under lower temperature is mainly caused by stronger intermolecular force of PVC. Owing to stronger inte..
Particle Size 900 µm
900 µm
<2%
Shandong Rike Chemical HELIâ„¢ HLC-2235 PVC Impact Modifier-CPE Series
Mechanism of Impact ModificationIt is found by research that the weak impact strength of PVC under lower temperature is mainly caused by stronger intermolecular force of PVC. Owing to stronger inte..
Particle Size 900 µm
900 µm
<2%
Shandong Rike Chemical HELIâ„¢ HLC-3235 PVC Impact Modifier-CPE Series
Mechanism of Impact ModificationIt is found by research that the weak impact strength of PVC under lower temperature is mainly caused by stronger intermolecular force of PVC. Owing to stronger inte..
Particle Size 900 µm
900 µm
<2%
Shandong Rike Chemical HELIâ„¢ HLC-40B PVC Impact Modifier-CPE Series
Mechanism of Impact ModificationIt is found by research that the weak impact strength of PVC under lower temperature is mainly caused by stronger intermolecular force of PVC. Owing to stronger inte..
Particle Size 900 - 1400 µm
900 - 1400 µm
Polimeri Europa Extir® D 5000 AE Expandable Polystyrene - Flame Retardant
Product Description:Extir D 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does not conta..