Polymer Property : Particle Size = 60 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 30 - 60 µm
30 - 60 µm
mesh.
Oceanchem Group Calcium Chloride 94-95% powder
Molecular Formula: CaCl2Information Provided by Oceanchem Group
Particle Size 35 - 60 µm
35 - 60 µm
average
Momentive Performance Materials PolarTherm® PT110 Boron Nitride (BN) Powder
Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarThermâ„¢'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp..
Particle Size 50 - 60 µm
50 - 60 µm
90%
H.C. Starck Amperit® 105.074 Agglomerated Sintered Molybdenum (Mo)
Particle Size 50 - 60 µm
50 - 60 µm
90%
H.C. Starck Amperit® 538.074 Agglomerated, Sintered Tungsten Carbide-Tungsten Boride-Cobalt (WC-WB-Co ) 60-30-10
Particle Size 50 - 60 µm
50 - 60 µm
90%
H.C. Starck Amperit® 559.074 Agglomerated, Sintered Tungsten Carbide-Cobalt-Chromium 86-6-8 (WC-Co-Cr)
Particle Size 52 - 60 µm
52 - 60 µm
90%
H.C. Starck Amperit® 586.1 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr)
Particle Size 40 - 60 µm
40 - 60 µm
Lucite International Colacryl ® D150 Acrylic Dental Resin
A range of Methyl Methacrylate polymers designed for use as standard heat-curing denture base resins.Features: Fine free-flowing bead polymers containing residual peroxide initiator; Curing cycles f..
Particle Size 50 - 60 µm
50 - 60 µm
Lucite International Colacryl ® D80FC Acrylic Dental Resin
Methyl Methacrylate polymers and copolymers designed for use as fast heat curing denture base resins.Colacryl denture base resins feature fast polymerisation and a wide choice of process properties...
Particle Size 50 - 60 µm
50 - 60 µm
Lucite International Colacryl ® TS2050 Acrylic Resin
Lucite® Colacryl® TS2050 is a hard, methyl methacrylate based, acrylic resin with an especially tight particle size distribution, leading to extremely good performance in glass separation appl..
Particle Size 50 - 60 µm
50 - 60 µm
90%
H.C. Starck Amperit® 140.3 Tungsten (W)
HS Number: 81011000
Particle Size 50 - 60 µm
50 - 60 µm
90%
H.C. Starck Amperit® 146.3 Chromium (Cr)
HS Number: 81122031
Particle Size 20 - 60 µm
20 - 60 µm
DayGlo ZQ Pigments ZQ-11 Aurora Pink
DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar..
Particle Size 20 - 60 µm
20 - 60 µm
DayGlo ZQ Pigments ZQ-12 Neon Red
DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar..
Particle Size 20 - 60 µm
20 - 60 µm
DayGlo ZQ Pigments ZQ-13 Rocket Red
DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar..
Particle Size 20 - 60 µm
20 - 60 µm
DayGlo ZQ Pigments ZQ-14 Fire Orange
DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar..
Particle Size 20 - 60 µm
20 - 60 µm
DayGlo ZQ Pigments ZQ-15 Blaze Orange
DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar..
Particle Size 20 - 60 µm
20 - 60 µm
DayGlo ZQ Pigments ZQ-16 Arc Yellow
DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar..
Particle Size 20 - 60 µm
20 - 60 µm
DayGlo ZQ Pigments ZQ-17 Saturn Yellow
DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar..
Particle Size 20 - 60 µm
20 - 60 µm
DayGlo ZQ Pigments ZQ-18 Signal Green
DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar..
Particle Size 20 - 60 µm
20 - 60 µm
DayGlo ZQ Pigments ZQ-19 Horizon Blue
DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar..
Particle Size 20 - 60 µm
20 - 60 µm
DayGlo ZQ Pigments ZQ-21 Corona Magenta
DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar..