Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucite International Colacryl ® D80FC Acrylic Dental Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Colacryl ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Colacryl ® D80FC Acrylic Dental Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Methyl Methacrylate polymers and copolymers designed for use as fast heat curing denture base resins.Colacryl denture base resins feature fast polymerisation and a wide choice of process properties. The resins are designed to meet the requirements of BS 2487:1989/BSEN ISO 1567.Benefits: Short cure cycles, Easy mixing, Good clarity, Excellent pigment acceptance.Information provided by Lucite International
Physical Properties Metric English Comments
Particle Size 50 - 60 µm
50 - 60 µm
Molecular Weight 1.50e+6 - 2.00e+6 g/mol
1.50e+6 - 2.00e+6 g/mol
Descriptive Properties Value Comments
Residual peroxide (%) .25 - .32
Work Time (min) 15
Users viewing this material also viewed the following: