TIMCAL TIMREX® KC44 Primary Synthetic Graphite

Category Carbon , Graphite , Other Engineering Material , Additive/Filler for Polymer
Manufacturer TIMCAL
Trade Name TIMREX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TIMCAL TIMREX® KC44 Primary Synthetic Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all production and processing stages, strict final inspection, and clearly defined development processes.TIMREX Primary Synthetic Graphite shows unique properties thanks to the combination of a consistent purity, perfect crystalline structure and well defined texture.Information provided by TIMCAL
Physical Properties Metric English Comments
Bulk Density 0.190 g/cc
0.00686 lb/in³
Scott
Particle Size 48 µm
48 µm
d90
Specific Surface Area 7.0 m²/g
7.0 m²/g
BET
Ash 0.050 %
0.050 %
Typical
Electrical Properties Metric English Comments
Electrical Resistivity 125 ohm-cm
125 ohm-cm
8% graphite
200 ohm-cm
200 ohm-cm
6.5% graphite
400 ohm-cm
400 ohm-cm
5.3% graphite
500 ohm-cm
500 ohm-cm
4.8% graphite
Descriptive Properties Value Comments
Aspect Fine black powder
Battery type High-drain C, D
Flexural Strength 7 N
4.7% graphite
7.5 N
4.7% graphite
8 N
4.7% graphite
8.5 N
4.7% graphite
Graphite 6-8%
Recommended concentration
Particle Shape Isometric, irregular spheroids