Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 37 - 52 µm | 37 - 52 µm | d90, Guaranteed |
TIMCAL TIMREX® T44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 48 - 52 µm | 48 - 52 µm | Average; ATO 40-41-0 (Coulter Counter) |
Arkema Group ORGASOL® 2002 ES 5 Nat 3 Polyamide 12 Information provided by Arkema Group |