Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 30 - 40 µm | 30 - 40 µm | Average; for outer type spray system; Microtrac HRA |
NYC YT3WBHQ Y2O3 Powder for Spray Coating High purity granules produced in clean environment. Uses include semiconductor / LCD industries and electroceramics.Narrow particle size distributionTailorable for each spray coating technologyNo c.. |
|||
Particle Size | 36 - 40 µm | 36 - 40 µm | 90% |
H.C. Starck Amperit® 151.065 Tantalum (Ta) |
|||
Particle Size | 36 - 40 µm | 36 - 40 µm | 90% |
H.C. Starck Amperit® 161.065 Niobium (Nb) |
|||
Particle Size | 32 - 40 µm | 32 - 40 µm | 50% |
H.C. Starck Amperit® 554.074 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr) |
|||
Particle Size | 32 - 40 µm | 32 - 40 µm | 50% |
H.C. Starck Amperit® 586.054 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr) |
|||
Particle Size | 30 - 40 µm | 30 - 40 µm | 90% |
H.C. Starck Amperit® 588.059 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) |
|||
Particle Size | 30 - 40 µm | 30 - 40 µm | 50% |
H.C. Starck Amperit® 832.054 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Particle Size | 30 - 40 µm | 30 - 40 µm | Blue |
Solvay Chemicals Blue pigment Information provided by Solvay |
|||
Particle Size | 20 - 40 µm | 20 - 40 µm | D(0.5) |
Akzo Nobel Expancel® 051 DE 40 d60 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 20 - 40 µm | 20 - 40 µm | D(0.5) |
Akzo Nobel Expancel® 461 DE 40 d60 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 30 - 40 µm | 30 - 40 µm | 90% |
H.C. Starck Amperit® 529.053 Tungsten Carbide - Hastalloy C 85-15 (NiMoCrFeCo) |