NYC YT3WBHQ Y2O3 Powder for Spray Coating

Category Ceramic , Oxide
Manufacturer Nippon Yttrium Company (NYC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NYC YT3WBHQ Y2O3 Powder for Spray Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High purity granules produced in clean environment. Uses include semiconductor / LCD industries and electroceramics.Narrow particle size distributionTailorable for each spray coating technologyNo clogging in high efficiency spray coating
Physical Properties Metric English Comments
Bulk Density 1.40 - 1.60 g/cc
0.0506 - 0.0578 lb/in³
JIS K5101
Loss On Ignition <= 0.500 %

@Temperature 1000 °C,
Time 3600 sec
<= 0.500 %

@Temperature 1830 °F,
Time 1.00 hour
Particle Size 30 - 40 µm
30 - 40 µm
Average; for outer type spray system; Microtrac HRA
40 - 50 µm
40 - 50 µm
Average; for inner type spray system; Microtrac HRA
Component Elements Properties Metric English Comments
Fe2O3 <= 0.0020 %
<= 0.0020 %
ICP-AES
Na2O <= 0.0010 %
<= 0.0010 %
AA
Y2O3 >= 99.99 %
>= 99.99 %
TREO
Descriptive Properties Value Comments
Angle of Repose 24 - 26°
JIS K5101