H.C. Starck Amperit® 529.053 Tungsten Carbide - Hastalloy C 85-15 (NiMoCrFeCo)

Category Ceramic , Carbide
Manufacturer H.C. Starck
Trade Name Amperit®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Amperit® 529.053 Tungsten Carbide - Hastalloy C 85-15 (NiMoCrFeCo).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 3.80 - 4.60 g/cc
0.137 - 0.166 lb/in³
ASTM B417
Particle Size 9.0 - 13 µm
9.0 - 13 µm
10%
18 - 24 µm
18 - 24 µm
50%
30 - 40 µm
30 - 40 µm
90%
44 µm
44 µm
96% less than
62 µm
62 µm
99% less than
88 µm
88 µm
100% less than
Component Elements Properties Metric English Comments
Carbon, C 5.0 - 6.0 %
5.0 - 6.0 %
Chromium, Cr 2.0 - 3.5 %
2.0 - 3.5 %
Cobalt, Co 0.30 - 0.60 %
0.30 - 0.60 %
Iron, Fe 0.80 - 1.5 %
0.80 - 1.5 %
Molybdenum, Mo 2.0 - 3.5 %
2.0 - 3.5 %
Nickel, Ni 8.0 - 12 %
8.0 - 12 %
Oxygen, O <= 0.20 %
<= 0.20 %