Polymer Property : Particle Size = 32 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size <= 32 µm
<= 32 µm
90% smaller than
Nyco M325 WOLLASTOCOAT® Wollastonite
Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br..
Particle Size 32 µm
32 µm
Average Diameter
Potters Industries Conduct-O-Fil® S3000-S2E Silver-Coated Solid Glass Spheres
Conduct-O-Fil® Conductive Particles are engineered to meet a broad range of conductive and electro magnetic interference requirements. Applications include EMI shielding, conductive adhesives, Z-a..
Particle Size 32 µm
32 µm
Average Diameter
Potters Industries Conduct-O-Fil® S3000-S3E Silver-Coated Solid Glass Spheres
Conduct-O-Fil® Conductive Particles are engineered to meet a broad range of conductive and electro magnetic interference requirements. Applications include EMI shielding, conductive adhesives, Z-a..
Particle Size 32 µm
32 µm
20% max, wet sieve
Magyar Aluminum ALO-P90-06 Alumina
Alumina for Polishing
Particle Size 32 - 44 µm
32 - 44 µm
d90
Indium Corp. Standard ITO Indium Tin Oxide
Indium Tin Oxide (ITO, or tin-doped indium oxide) is a mixture of indium(III) oxide and tin(IV) oxide, typically 90% indium oxide, 10% tin oxide by weight. In powder form it is yellow-green in colo..
Particle Size 32 - 42 µm
32 - 42 µm
50%
H.C. Starck Amperit® 140.1 Tungsten (W)
HS Number: 81011000
Particle Size 32 - 38 µm
32 - 38 µm
50%
H.C. Starck Amperit® 526.062 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17
Particle Size 32 - 38 µm
32 - 38 µm
50%
H.C. Starck Amperit® 526.074 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17
Particle Size 32 - 40 µm
32 - 40 µm
50%
H.C. Starck Amperit® 554.074 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)
Particle Size 32 µm
32 µm
Maximum of 12% less than for Ni-SF RC 60
H.C. Starck Amperit® 560.062 Tungsten Carbide-Cobalt(83-17)-Nickel-SF RC 60 50-50 (Wc-Co / NiSF RC 60)
Composition is of NiSF RC 60 only
Particle Size 32 - 38 µm
32 - 38 µm
50% for WC-Co 83-17
H.C. Starck Amperit® 560.062 Tungsten Carbide-Cobalt(83-17)-Nickel-SF RC 60 50-50 (Wc-Co / NiSF RC 60)
Composition is of NiSF RC 60 only
Particle Size 32 µm
32 µm
Maximum of 7% less than, WSC-Ni 92/8
H.C. Starck Amperit® 568.005 Tungsten Carbide-Nickel 92-8 - Nickel SF RC 60 65-35
Composition is of NiSF RC 60 only
Particle Size 32 - 40 µm
32 - 40 µm
50%
H.C. Starck Amperit® 586.054 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr)
Particle Size 32 - 48 µm
32 - 48 µm
Lucite International Colacryl ® D1-120 Acrylic Dental Resin
Cold-curing denture repair resin with Methyl Methacrylate based copolymers. Features fast polymerisation, easy mixing, good clarity, short hydroflask cure cycles, and excellent pigment acceptance.I..
Particle Size <= 32 µm
<= 32 µm
74%
SGL Carbon Group CF 1135 Carbon Filler
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Particle Size <= 32 µm
<= 32 µm
67%
SGL Carbon Group CF 270 Graphite Filler
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Particle Size <= 32 µm
<= 32 µm
78%
SGL Carbon Group CF 3100 Graphite Filler
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Particle Size <= 32 µm
<= 32 µm
57%
SGL Carbon Group CF 480 Graphite Filler
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Particle Size <= 32 µm
<= 32 µm
60%
SGL Carbon Group CF 5250 Carbon Filler
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Particle Size 32 µm
32 µm
@ 98%
CIMBAR RiverCal™ 8107 & 8107C Calcium Carbonate (CaCO3)
RiverCal™ 8100 Series Calcium Carbonate are high purity, white, functional fillers targeted for use in thermosets, thermoplastics, paint & coatings, sealants, TPO's and TPE's and other applications..