Physical Properties Metric English Comments
Particle Size 26 - 34 µm
26 - 34 µm
90%
H.C. Starck Amperit® 519.059 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO)
Particle Size 28 - 34 µm
28 - 34 µm
50%
H.C. Starck Amperit® 538.074 Agglomerated, Sintered Tungsten Carbide-Tungsten Boride-Cobalt (WC-WB-Co ) 60-30-10
Particle Size 26 - 34 µm
26 - 34 µm
90%
H.C. Starck Amperit® 558.059 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)
Particle Size 28 - 34 µm
28 - 34 µm
50%
H.C. Starck Amperit® 559.074 Agglomerated, Sintered Tungsten Carbide-Cobalt-Chromium 86-6-8 (WC-Co-Cr)
Particle Size 26 - 34 µm
26 - 34 µm
50%
H.C. Starck Amperit® 552.074 Tungsten Carbide - Chromium Carbide-Nickel 73-20-7 (WC-CrC-Ni)
Particle Size 26 - 34 µm
26 - 34 µm
90%
H.C. Starck Amperit® 526.059 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17
Particle Size 26 - 34 µm
26 - 34 µm
90%
H.C. Starck Amperit® 547.002 Tungsten Carbide-Nickel 88-12 (WC-Ni)
Particle Size 26 - 34 µm
26 - 34 µm
90%
H.C. Starck Amperit® 551.059 Tungsten Carbide - Chromium Carbide - Nickel 70-20-7 (W-CrC-Ni)