Potters Industries Sphericel® 60P18 Hollow Glass Spheres

Category Ceramic , Glass , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Potters Industries
Trade Name Sphericel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Potters Industries Sphericel® 60P18 Hollow Glass Spheres.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: This microsphere is strong with a density of 0.6g/cc, and has the added advantage of a very small particle size of only 18 micron (mean). Fused glass, hollow spheres used as an additive for thermoplastic and thermosetting resin systems.Information provided by Potters Industries.
Physical Properties Metric English Comments
Density 0.600 g/cc
0.0217 lb/in³
true density of spheres
Particle Size 6.0 - 10 µm
6.0 - 10 µm
10% finer than
15 - 19 µm
15 - 19 µm
50% finer than
16 - 20 µm
16 - 20 µm
mean value
28 - 32 µm
28 - 32 µm
90% finer than
Descriptive Properties Value Comments
Appearance white powder
Composition Fused Inorganic Oxides
Strength (% volume loss) 0.1
11000 psi