Solvay MIRAPOL® SURF-S 411 HA Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name MIRAPOL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay MIRAPOL® SURF-S 411 HA Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Rinse aid polymer specially formulated for auto dish wash powders and tablets. Recommended as a substitute to rinse aid surfactants. Enables raw material cost saving, while boosting rinse aid performance.Identification: BLEND OF ACRYLIC BASED POLYMER AND SODIUM TRIPOLYPHOSPHATE.Use level : 5 – 10% as isAvailable in: Asia Pacific, Europe, Latin America and North America Applications: Polymer to be used in automatic dish washing (3 in 1 tablets or powders) to deliver the rinse aid function..Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Bulk Density 1.00 - 1.20 g/cc
0.0361 - 0.0434 lb/in³
540MA3C63
Particle Size <= 100 µm
<= 100 µm
3% Max; 540MA3C5E
>= 1600 µm
>= 1600 µm
2% Max; 540MA3C5E
Processing Properties Metric English Comments
Moisture Content 6.0 - 8.5 %

@Temperature 180 °C,
Time 3600 sec
6.0 - 8.5 %

@Temperature 356 °F,
Time 1.00 hour
540MA3C63
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance White powder
540MA3C1F
Composition COD method Actives
2.2-2.6%, 540MO3C10
STPP content
89-92%
Preservative 1,2-benzisothiazol-3(2H)-one
0.00015
2-methyl-2H-isothiazol-3-one
0.00015
3-Iodo-2-propynyl butylcarbamate
6E-05