Material Notes:
PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surface just prior to the molding of SMC/BMC. Applications can be found in sanitary products such as kitchen sinks and shower trays. A special, appealing color effect is created by mixing different colors, which gives a speckle effectInformation provided by Raschig Group
Physical Properties Metric English Comments
Specific Gravity 1.30 - 1.50 g/cc
1.30 - 1.50 g/cc
Bulk Density 0.600 - 0.700 g/cc
0.0217 - 0.0253 lb/in³
Particle Size 10.0 - 25.0 µm
10.0 - 25.0 µm
D 0.1, SATP-114, Malvern method
50.0 - 75.0 µm
50.0 - 75.0 µm
D 0.5, SATP-114, Malvern method
100 - 175 µm
100 - 175 µm
D 0.9, SATP-114, Malvern method
Storage Temperature <= 20.0 °C
<= 68.0 °F
Mechanical Properties Metric English Comments
Elongation at Break 2.00 - 5.00 %
2.00 - 5.00 %
ASTM D790
Flexural Strength 30.0 - 60.0 MPa
4350 - 8700 psi
ASTM D790
Flexural Modulus 5.00 - 10.0 GPa
725 - 1450 ksi
ASTM D790
Abrasion <= 0.500

@Load 0.500 kg
<= 0.500

@Load 1.10 lb
[g] S42 paper, 500 turns; DIN 53799
Optical Properties Metric English Comments
Gloss 50.0 %
50.0 %
20°
75.0 %
75.0 %
60°
90.0 %
90.0 %
85°
Processing Properties Metric English Comments
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Brabender cycle time 75-115 s
150°C, SATP-104
Powder stability >8 hrs
30°C, SATP-128
Scratch resistance >2 N
DIN 53799