Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 110 - 150 µm | 110 - 150 µm | Median Granulate Size |
Nabaltec GRANALOX® NM 9212 F Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Particle Size | 5.0 - 150 µm | 5.0 - 150 µm | range |
Potters Industries Q-Cel® 5019 Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat.. |
|||
Particle Size | 5.0 - 150 µm | 5.0 - 150 µm | |
Potters Industries Q-Cel® 5032S Hollow Engineered Glass Microspheres Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me.. |
|||
Particle Size | 5.0 - 150 µm | 5.0 - 150 µm | |
Potters Industries Q-Cel® 6019S Hollow Engineered Glass Microspheres Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me.. |
|||
Particle Size | 5.0 - 150 µm | 5.0 - 150 µm | range |
Potters Industries Q-Cel® 6028 Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat.. |
|||
Particle Size | 5.0 - 150 µm | 5.0 - 150 µm | |
Potters Industries Q-Cel® 7019 Hollow Engineered Glass Microspheres Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me.. |
|||
Particle Size | 120 - 150 µm | 120 - 150 µm | Laser Light Scattering Method; LSY-QB-ID016 |
LG Chemical Lutex 120 NBR Latex Description: Tensile strength, Elongation, Oil resistance, Abrasion resistance, Excellent elasticity, WhitenessApplication: Nitrile Glove (Examination Glove, Clean Room Glove), Supported Glove (Indu.. |
|||
Particle Size | 100 - 150 µm | 100 - 150 µm | Mean particle size is 100 to 150 µm. Crystal size is 10 µm. |
Momentive Performance Materials AC-6028 Boron Nitride (BN) Powder Grade AC-6028 consists of agglomerated particles of hexagonal Boron Nitride (BN) with a mean particle size between 100 and 150µ. It exhibits the unique properties of BN in a form readily used in.. |
|||
Particle Size | 10 - 150 µm | 10 - 150 µm | |
SPHERE ONE EXTENDOSPHERESâ„¢ SL-150 Hollow Spheres EXTENDOSPHERESâ„¢ SL are white, low-cost, low-density ceramic hollow spheres.Applications: With a density of 0.73 g/cc and a crush strength of 3,000 psi, these hollow spheres are ideal for use in.. |
|||
Particle Size | 10 - 150 µm | 10 - 150 µm | |
SPHERE ONE EXTENDOSPHERESâ„¢ TG Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Particle Size | 10 - 150 µm | 10 - 150 µm | |
SPHERE ONE EXTENDOSPHERESâ„¢ XOL-150 Hollow Spheres EXTENDOSPHERESâ„¢ XOL-150 are white aluminosilicate multicellular hollow spheres. The density of this product is 0.30 g/cc. In plastic and coating applications, EXTENDOSPHERESâ„¢ XOL-150 hollo.. |
|||
Particle Size | 75 - 150 µm | 75 - 150 µm | > 99 wt.%; DIN EN ISO 4610 |
Suzhou Hipro Polymers Hiprolon® 11 PFB Colorized Nylon powder Hiprolon® 11 PFB colorized is a fluid-bed polyamide powder partly comprised of bio-renewable raw materials. It has excellent weather ability, chemical resistance, wear resistance, impact resistan.. |
|||
Particle Size | 75 - 150 µm | 75 - 150 µm | > 99 wt.%; DIN EN ISO 4610 |
Suzhou Hipro Polymers Hiprolon® 11 PFB Colorized Nylon powder Hiprolon® 11 PFB colorized is a fluid-bed polyamide powder fully comprised of bio-renewable raw materials. It has excellent weather ability, chemical resistance, wear resistance, impact resistanc.. |
|||
Particle Size | 100 - 150 µm | 100 - 150 µm | average |
Momentive Performance Materials PolarTherm® PT350 Boron Nitride (BN) Powder Low Density BN AgglomerateWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic compon.. |
|||
Particle Size | 100 - 150 µm | 100 - 150 µm | |
Potters Industries A-Series P-0060 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |