Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.200 µm | 0.200 µm | Average Stokes Equivalent Diameter |
KaMin KaMin® HG Kaolin Clay - Waterwashed KaMin® HG is an economical, general purpose, water-washed kaolin with fine particle size and intermediate brightness. It is suitable for water borne paint, ink and adhesive applications.Industry:.. |
|||
Particle Size | 0.200 µm | 0.200 µm | Average Stokes Equivalent Diameter |
KaMin KaMin® HG90 Kaolin Clay - Ultrafine, high brightness KaMin® HG90 is a high brightness, ultra-fine particle size, platy kaolin with moderate water demand providing good tinting strength, Ti02 extension and gloss in water based paints. KaMin® HG90.. |
|||
Particle Size | 0.200 µm | 0.200 µm | Average Stokes Equivalent Diameter |
KaMin Nucap® 100G Kaolin Clay - Surface Treated Cost effective, moderate brightness, mercapto silane treated clay for partial thermal black replacement.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl Rubber, EP.. |
|||
Particle Size | 0.200 µm | 0.200 µm | Average Stokes Equivalent Diameter |
KaMin Nucap® 190W Kaolin Clay - Surface Treated Reinforcing filler/extender for elastomeric systems. Nucap®190W is a high brightness treated kaolin used in white roofing membranes and white sidewalls. Silane treated clays mix in quicker and ma.. |
|||
Particle Size | 0.200 µm | 0.200 µm | Average Stokes Equivalent Diameter |
KaMin Nucap® 290W Kaolin Clay - Surface Treated Reinforcing filler/extender for elastomeric systems. Nucap®290W is a high brightness kaolin with the highest level of surface treatment to impart the best mechanical properties and water resistan.. |
|||
Particle Size | 0.200 µm | 0.200 µm | Average Stokes Equivalent Diameter |
KaMin Nulok® 390 Kaolin Clay - Surface Treated High brightness, ultra-fine kaolin extender for white or bright colored rubber or plastic, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl R.. |
|||
Particle Size | 0.200 µm | 0.200 µm | Average Stokes Equivalent Diameter |
KaMin Polygloss® 90 Kaolin Clay - Ultrafine, high brightness Ultrafine, highly pulverized, premium brightness kaolin for extending high gloss solvent and water-based coatings.Industry: Paint & Coatings, Rubber & Plastic, InkUses: Architectural Coatings, Indus.. |
|||
Particle Size | 0.200 µm | 0.200 µm | Average Stokes Equivalent Diameter |
KaMin Polyfil® HG Kaolin Clay - Waterwashed Polyfil® HG is an ultra-fine particle size, moderate brightness water washed kaolin clay. It offers acid resistance, barrier properties, reinforcement, neutral ph, and extremely low crystalline .. |
|||
Particle Size | 0.200 µm | 0.200 µm | Average Stokes Equivalent Diameter |
KaMin Polyfil® HG90 Kaolin Clay - Waterwashed High brightness, ultra-fine kaolin extender for white or bright colored rubber or plastic, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl R.. |