Material Notes:
Polyfil® HG is an ultra-fine particle size, moderate brightness water washed kaolin clay. It offers acid resistance, barrier properties, reinforcement, neutral ph, and extremely low crystalline silica and salt content. Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl Rubber, General Plastics, Nylon, Thermoset, Thermoplastic, EPDM, Masterbatch, Wire & CableInformation provided by KaMin LLC.
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Bulk Density 0.801 - 0.897 g/cc
0.0289 - 0.0324 lb/in³
Loose
Solids Content 69.5 - 71 %
69.5 - 71 %
Slurry
Brightness 87.5 - 88.5 %
87.5 - 88.5 %
Reflectance (TAPPI)
Oil Absorption 33 %
33 %
Fineness >= 5
>= 5
Hegman Grind
Moisture Absorption at Equilibrium <= 1.5 %
<= 1.5 %
As Produced
Particle Size 0.200 µm
0.200 µm
Average Stokes Equivalent Diameter
0.500 µm
0.500 µm
Median (Malvern Laser)
Particle Mesh Size 325 Mesh
325 Mesh
0.005% Retained
pH 6 - 8
6 - 8
100 g/250 ml H2O Slurry
Specific Surface Area 21.0 m²/g
21.0 m²/g
BET
Brookfield Viscosity 450 cP

@Temperature 25.0 °C
450 cP

@Temperature 77.0 °F
20 RPM
Descriptive Properties Value Comments
Bulking Value 21.7 lb.gal
CAS Number 1332-58-7
Crystalline Silica (quartz) <0.1%
Physical Forms Dry, Slurry
Shipping Point Wrens, GA