Material Notes:
Ultrafine, highly pulverized, premium brightness kaolin for extending high gloss solvent and water-based coatings.Industry: Paint & Coatings, Rubber & Plastic, InkUses: Architectural Coatings, Industrial Coatings, Wood Coatings, Satin, Gloss, Powder Coatings, Primer, Tinting Paste, Pigmented Coatings, Non-Black Rubber, General Plastics, Thermoset Plastic, Masterbatch, Lithographic/Offset, Sheetfed, Web Offset Heatset, Web Offset Coldset, Gravure Solvent Borne, Flexo Solvent Borne, Screen, LetterpressInformation provided by KaMin LLC.
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Bulk Density 0.160 - 0.192 g/cc
0.00579 - 0.00694 lb/in³
Loose
Brightness 91 %
91 %
Reflectance (TAPPI)
Oil Absorption 42 %
42 %
Fineness >= 7
>= 7
Hegman Grind
Moisture Absorption at Equilibrium <= 1 %
<= 1 %
As Produced
Particle Size 0.200 µm
0.200 µm
Average Stokes Equivalent Diameter
0.400 µm
0.400 µm
Median (Malvern Laser)
Particle Mesh Size 325 Mesh
325 Mesh
0.005% Retained
pH 7
7
100 g/250 ml H2O Slurry
Specific Surface Area 22.0 m²/g
22.0 m²/g
BET
Descriptive Properties Value Comments
Bulking Value 21.7 lb.gal
CAS Number 1332-58-7
Crystalline Silica (quartz) <0.1%
Physical Form Dry
Shipping Point Wrens, GA