Physical Properties Metric English Comments
Particle Size 0.200 µm
0.200 µm
Average Stokes Equivalent Diameter
KaMin KaMin® HG Kaolin Clay - Waterwashed
KaMin® HG is an economical, general purpose, water-washed kaolin with fine particle size and intermediate brightness. It is suitable for water borne paint, ink and adhesive applications.Industry:..
Particle Size 0.200 µm
0.200 µm
Average Stokes Equivalent Diameter
KaMin KaMin® HG90 Kaolin Clay - Ultrafine, high brightness
KaMin® HG90 is a high brightness, ultra-fine particle size, platy kaolin with moderate water demand providing good tinting strength, Ti02 extension and gloss in water based paints. KaMin® HG90..
Particle Size 0.200 µm
0.200 µm
Average Stokes Equivalent Diameter
KaMin Nucap® 100G Kaolin Clay - Surface Treated
Cost effective, moderate brightness, mercapto silane treated clay for partial thermal black replacement.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl Rubber, EP..
Particle Size 0.200 µm
0.200 µm
Average Stokes Equivalent Diameter
KaMin Nucap® 190W Kaolin Clay - Surface Treated
Reinforcing filler/extender for elastomeric systems. Nucap®190W is a high brightness treated kaolin used in white roofing membranes and white sidewalls. Silane treated clays mix in quicker and ma..
Particle Size 0.200 µm
0.200 µm
Average Stokes Equivalent Diameter
KaMin Nucap® 290W Kaolin Clay - Surface Treated
Reinforcing filler/extender for elastomeric systems. Nucap®290W is a high brightness kaolin with the highest level of surface treatment to impart the best mechanical properties and water resistan..
Particle Size 0.200 µm
0.200 µm
Average Stokes Equivalent Diameter
KaMin Nulok® 390 Kaolin Clay - Surface Treated
High brightness, ultra-fine kaolin extender for white or bright colored rubber or plastic, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl R..
Particle Size 0.200 µm
0.200 µm
Average Stokes Equivalent Diameter
KaMin Polygloss® 90 Kaolin Clay - Ultrafine, high brightness
Ultrafine, highly pulverized, premium brightness kaolin for extending high gloss solvent and water-based coatings.Industry: Paint & Coatings, Rubber & Plastic, InkUses: Architectural Coatings, Indus..
Particle Size 0.200 µm
0.200 µm
Average Stokes Equivalent Diameter
KaMin Polyfil® HG Kaolin Clay - Waterwashed
Polyfil® HG is an ultra-fine particle size, moderate brightness water washed kaolin clay. It offers acid resistance, barrier properties, reinforcement, neutral ph, and extremely low crystalline ..
Particle Size 0.200 µm
0.200 µm
Average Stokes Equivalent Diameter
KaMin Polyfil® HG90 Kaolin Clay - Waterwashed