KaMin KaMin® HG90 Kaolin Clay - Ultrafine, high brightness

Category Ceramic , Clay , Kaolin Clay
Manufacturer KaMin LLC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KaMin KaMin® HG90 Kaolin Clay - Ultrafine, high brightness.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KaMin® HG90 is a high brightness, ultra-fine particle size, platy kaolin with moderate water demand providing good tinting strength, Ti02 extension and gloss in water based paints. KaMin® HG90 is ideally suited for water-borne paint and ink applications, where high brightness and whiteness are important.Industry: Paint & Coatings, Adhesives & Sealants, InkUses: Architectural Coatings, Industrial Coatings, Wood Coatings, Satin, Gloss, Water Based, Gravure Water Based, Flexo Water BasedInformation provided by KaMin LLC.
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Bulk Density 0.801 - 0.897 g/cc
0.0289 - 0.0324 lb/in³
Loose
Solids Content 69.5 - 71 %
69.5 - 71 %
Slurry
Brightness 90 - 91.5 %
90 - 91.5 %
Reflectance (TAPPI)
Oil Absorption 42 %
42 %
Fineness >= 5
>= 5
Hegman Grind
Moisture Absorption at Equilibrium <= 1.5 %
<= 1.5 %
As Produced
Particle Size 0.200 µm
0.200 µm
Average Stokes Equivalent Diameter
0.400 µm
0.400 µm
Median (Malvern Laser)
Particle Mesh Size 325 Mesh
325 Mesh
0.005% Retained
pH 6 - 8
6 - 8
100 g/250 ml H2O Slurry
Specific Surface Area 21.0 m²/g
21.0 m²/g
BET
Brookfield Viscosity 450 cP

@Temperature 25.0 °C
450 cP

@Temperature 77.0 °F
20 RPM
Descriptive Properties Value Comments
Bulking Value 21.7 lb.gal
CAS Number 1332-58-7
Crystalline Silica (quartz) <0.1%
Physical Forms Dry, Slurry
Shipping Point Wrens, GA