Physical Properties Metric English Comments
Bulk Density 0.449 - 0.497 g/cc
0.0162 - 0.0179 lb/in³
Loose
KaMin KaMin® 35 Kaolin Clay - Waterwashed
Coarse kaolin, milled powder, with the lowest oil absorption, for extending without thickening.Industry: Paint & Coatings, Adhesives & SealantsUses: Architectural Coatings, Industrial Coatings, Wood..
Bulk Density 0.449 - 0.497 g/cc
0.0162 - 0.0179 lb/in³
Loose
KaMin Polyfil® 35 Kaolin Clay - Waterwashed
Coarse kaolin, with the lowest oil absorption, for extending without reinforcement, milled powder form.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, General Plastics, SMC/B..