Material Notes:
Gem-Tone™ Sapphire Blue is a rich blue colorant intended for use in clarified polypropylene. Clean, haze free, non-warping color formulations can easily be achieved with the use of this colorant. No blooming, migration or plateout problems will be seen with Gem-Tone colorants. These materials can be incorporated into polyolefin resins at levels as low as 0.05% and can be increased to higher levels to achieve the desired effect. Gem-Tone GC-19F Sapphire Blue is FDA approved for use in PP at levels NTE 0.1%.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Bulk Density 0.449 g/cc
0.0162 lb/in³
Oil Absorption 46 %
46 %
Particle Size 20 - 80 µm
20 - 80 µm
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Softening Point 110 - 135 °C
230 - 275 °F
Glass Transition Temp, Tg 103 °C
217 °F
Decomposition Temperature 315 °C
599 °F
Processing Properties Metric English Comments
Processing Temperature >= 177 °C
>= 350 °F
Descriptive Properties Value Comments
λmax 596nm
Abs. = 21000
644nm
Abs. = 23000
Users viewing this material also viewed the following: