KaMin KaMin® 35 Kaolin Clay - Waterwashed

Category Ceramic , Clay , Kaolin Clay
Manufacturer KaMin LLC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KaMin KaMin® 35 Kaolin Clay - Waterwashed.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Coarse kaolin, milled powder, with the lowest oil absorption, for extending without thickening.Industry: Paint & Coatings, Adhesives & SealantsUses: Architectural Coatings, Industrial Coatings, Wood Coatings, Flat/Matte, Primer, Water Based, Solvent BorneInformation provided by KaMin LLC.
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Bulk Density 0.449 - 0.497 g/cc
0.0162 - 0.0179 lb/in³
Loose
Brightness 84 %
84 %
Reflectance (TAPPI)
Oil Absorption 27 %
27 %
Fineness >= 4
>= 4
Hegman Grind
Moisture Absorption at Equilibrium <= 1.5 %
<= 1.5 %
As Produced
Particle Size 4.00 µm
4.00 µm
Average Stokes Equivalent Diameter
7.00 µm
7.00 µm
Median (Malvern Laser)
Particle Mesh Size 325 Mesh
325 Mesh
0.03% Retained
pH 7
7
100 g/250 ml H2O Slurry
Specific Surface Area 9.40 m²/g
9.40 m²/g
BET
Descriptive Properties Value Comments
Bulking Value 21.7 lb.gal
CAS Number 1332-58-7
Crystalline Silica (quartz) <0.1%
Physical Form Dry
Shipping Point Macon, GA