Physical Properties Metric English Comments
Bulk Density 2.65 - 2.75 g/cc
0.0957 - 0.0994 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 180 B Dense Refractory Castable
Description: This high quality castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of Fe2O3, this castable can..
Bulk Density 2.65 - 2.75 g/cc
0.0957 - 0.0994 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 180 TF Dense Refractory Castable
Description: Curon 180 TF is a tabular alumina based castable, highly abrasion resistant, especially developed for application in the vacuum ladle treatment installation in the steel refinery.Remark..
Bulk Density 2.65 - 2.75 g/cc
0.0957 - 0.0994 lb/in³
After drying at 110°C
Gouda Vuurvast VIBRON 165 Dense Vibrating Refractory Castable
Description: Vibron 165 is a low cement castable based on andalusite and especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provide..
Bulk Density >= 2.65 g/cc
>= 0.0957 lb/in³
Dried at 110°C
Sharadaa Ceramics REFCAST 80 High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Bulk Density >= 2.65 g/cc
>= 0.0957 lb/in³
After Drying at 110°C
Sharadaa Ceramics ZAP 002 Smart Cast Application
Special Properties: Thermal Shock Slag ResistanceIndustry: SteelApplication: Pig Iron Laddle working LayerInformation provided by Sharadaa Ceramics Pvt. Ltd.
Bulk Density >= 2.65 g/cc
>= 0.0957 lb/in³
After Drying at 110°C
Sharadaa Ceramics ZAP 005 Smart Cast Application
Special Properties: Non-wetting, Slag and Hot Abrasion ResistanceIndustry: SteelApplication: Trough LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Bulk Density 2.65 - 2.75 g/cc
0.0957 - 0.0994 lb/in³
Chosun Refractories CUN-738 Nozzle Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.65 g/cc
0.0957 lb/in³
Chosun Refractories SAL70 Special Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.65 g/cc
0.0957 lb/in³
Chosun Refractories SB75 Bricks, Oxide Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.65 g/cc
0.0957 lb/in³
Chosun Refractories SB90S Bricks, Oxide Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.65 g/cc
0.0957 lb/in³
Chosun Refractories SBN-1 Bricks, Reaction Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.65 g/cc
0.0957 lb/in³
Chosun Refractories SBSN Bricks, Reaction Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.65 g/cc
0.0957 lb/in³
Chosun Refractories SC80 Bricks, Oxide Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.65 g/cc
0.0957 lb/in³
Chosun Refractories BTB-17 Casting Block
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.65 - 2.75 g/cc
0.0957 - 0.0994 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 185 T Dense Refractory Castable
Description: Curon 185 T is a very pure high alumina castable based on tabular alumina with very low Fe2O3 and SiO2 contents. Suitable for use in strongly reducing atmospheres.Remarks: These values ..