Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.65 g/cc
0.0957 lb/in³
Porosity 17 %
17 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.024525 GPa

@Temperature 250 °C
3.5571 ksi

@Temperature 482 °F
0.024525 GPa

@Temperature 1400 °C
3.5571 ksi

@Temperature 2550 °F
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 4.80 µm/m-°C

@Temperature 1000 °C
2.67 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
Fe2O3 1.1 %
1.1 %
SiC 81 %
81 %
Descriptive Properties Value Comments
Refractories Under Load(2kg/?,T2?) 1,600
Users viewing this material also viewed the following: