Material Notes:
Description: Curon 185 T is a very pure high alumina castable based on tabular alumina with very low Fe2O3 and SiO2 contents. Suitable for use in strongly reducing atmospheres.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.65 - 2.75 g/cc
0.0957 - 0.0994 lb/in³
After drying at 110°C
Particle Size <= 5000 µm
<= 5000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 12.0 - 18.0 MPa

@Temperature 1600 °C
1740 - 2610 psi

@Temperature 2910 °F
Cold Crushing Strength
17.0 - 23.0 MPa

@Temperature 100 °C
2470 - 3340 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.21 - 1.41 W/m-K

@Temperature 600 °C
8.40 - 9.79 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.28 - 1.48 W/m-K

@Temperature 1600 °C
8.88 - 10.3 BTU-in/hr-ft²-°F

@Temperature 2910 °F
1.34 - 1.54 W/m-K

@Temperature 100 °C
9.30 - 10.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
Maximum Service Temperature, Air 1870 °C
3400 °F
Shrinkage -0.500 - 0.500 %

@Temperature 1600 °C
-0.500 - 0.500 %

@Temperature 2910 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 97 %
97 %
CaO 2.5 %
2.5 %
Fe2O3 0.15 %
0.15 %
Na2O or K2O <= 0.35 %
<= 0.35 %
SiO2 0.15 %
0.15 %
Descriptive Properties Value Comments
ASTM Classification G
Material Consumption per 1 m3 2650 kg
Mixing Water 9-11 liters
per 100 kgs dry material