Material Notes:
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum are tailored to the application areas in which the material is used such as wear resistance, high temperature stability, good electrical insulation, thermal conductivity and corrosion resistance.Used in electrical insulating and polishable machinery parts, chemical resistant and ballistic ceramics.
Physical Properties Metric English Comments
Bulk Density 1.20 - 1.30 g/cc
0.0434 - 0.0470 lb/in³
Density 3.65 - 3.75 g/cc
0.132 - 0.135 lb/in³
Sintered Density
Moisture Absorption at Equilibrium 0.20 - 0.50 %
0.20 - 0.50 %
Loss On Ignition 6.5 %
6.5 %
Particle Size 110 - 150 µm
110 - 150 µm
Median Granulate Size
Thermal Properties Metric English Comments
Shrinkage 15.5 - 16.5 %
15.5 - 16.5 %
linear
Component Elements Properties Metric English Comments
Al2O3 92 %
92 %
Na2O 0.10 %
0.10 %
Processing Properties Metric English Comments
Sintering Temperature 1580 °C
2880 °F
1550 - 1650 °C
2820 - 3000 °F
Interval (dense ceramic parts)
Descriptive Properties Value Comments
Dwell Time hr. 2
Users viewing this material also viewed the following: