Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.0160 - 0.0350 g/cc | 0.000578 - 0.00126 lb/in³ | |
BASF E-por® 0.02 g/cc Density; Styrene and Ethylene (Europe) Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e.. |
|||
Bulk Density | 0.0160 - 0.0350 g/cc | 0.000578 - 0.00126 lb/in³ | |
BASF E-por® 0.025 g/cc Density; Styrene and Ethylene (Europe) Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e.. |
|||
Bulk Density | 0.0160 - 0.0350 g/cc | 0.000578 - 0.00126 lb/in³ | |
BASF E-por® 0.035 g/cc Density; Styrene and Ethylene (Europe) Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e.. |
|||
Bulk Density | 0.0290 - 0.0350 g/cc | 0.00105 - 0.00126 lb/in³ | |
BASF Neopolen® P 9335 MG 0.035 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Bulk Density | 0.0290 - 0.0350 g/cc | 0.00105 - 0.00126 lb/in³ | |
BASF Neopolen® P 9335 MG 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Bulk Density | 0.0290 - 0.0350 g/cc | 0.00105 - 0.00126 lb/in³ | |
BASF Neopolen® P 9335 MG 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Bulk Density | 0.0290 - 0.0350 g/cc | 0.00105 - 0.00126 lb/in³ | |
BASF Neopolen® P 9335 MG 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Bulk Density | 0.0290 - 0.0350 g/cc | 0.00105 - 0.00126 lb/in³ | |
BASF Neopolen® P 9335 MG 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Bulk Density | 0.0160 - 0.0350 g/cc | 0.000578 - 0.00126 lb/in³ | |
BASF E-por® 0.03 g/cc Density; Styrene and Ethylene (Europe) Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e.. |
|||
Bulk Density | 0.0180 - 0.0350 g/cc | 0.000650 - 0.00126 lb/in³ | |
BASF Styropor® KF 462M EPS Description: Expandable polystyrene (EPS) with pentane as a blowing agent. For the production of expanded foam. Block having bulk densities of 18-35 kg/m3 and fire characteristics in conformity with.. |