Material Notes:
Description: Expandable polystyrene (EPS) with pentane as a blowing agent. For the production of expanded foam. Block having bulk densities of 18-35 kg/m3 and fire characteristics in conformity with: DIN 4102-B1, KSM 3008 (Korea standard), GB/T 2406 (China Standard), UL94.Information provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.0180 - 0.0350 g/cc
0.000650 - 0.00126 lb/in³
Bead Size 0.640 - 0.680 mm
0.0252 - 0.0268 in
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
Descriptive Properties Value Comments
Commercial Status North America
Sieve Analysis <0.4 mm
max 1%
> 0.84 mm
max 1%
0.7 - 0.5 mm
min 98%