Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.0160 g/cc | 0.000578 lb/in³ | Minimum |
SYNTHOS Koplen® 0814 F Expandable Polystyrene Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to moldings and block.Specific Characteristics: Flammability .. |
|||
Bulk Density | 0.0160 - 0.0400 g/cc | 0.000578 - 0.00145 lb/in³ | Typical |
SYNTHOS Koplen® 0814 F Expandable Polystyrene Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to moldings and block.Specific Characteristics: Flammability .. |
|||
Bulk Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Typical |
SYNTHOS Koplen® 0814 FR Expandable Polystyrene Low Pentane Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to molded bricks and blocks. Lower density can be.. |
|||
Bulk Density | 0.0160 - 0.0350 g/cc | 0.000578 - 0.00126 lb/in³ | |
BASF E-por® 0.02 g/cc Density; Styrene and Ethylene (Europe) Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e.. |
|||
Bulk Density | 0.0160 - 0.0350 g/cc | 0.000578 - 0.00126 lb/in³ | |
BASF E-por® 0.025 g/cc Density; Styrene and Ethylene (Europe) Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e.. |
|||
Bulk Density | 0.0160 - 0.0350 g/cc | 0.000578 - 0.00126 lb/in³ | |
BASF E-por® 0.035 g/cc Density; Styrene and Ethylene (Europe) Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e.. |
|||
Bulk Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | |
BASF Styropor® KF 362M EPS Description: Expandable polystyrene (EPS) with pentane as a blowing agent. For the production of expanded foam. Block having bulk densities of 16-30 kg/m3 and fire characteristics in conformity with.. |
|||
Bulk Density | 0.0160 - 0.0350 g/cc | 0.000578 - 0.00126 lb/in³ | |
BASF E-por® 0.03 g/cc Density; Styrene and Ethylene (Europe) Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e.. |