Physical Properties Metric English Comments
Bulk Density 0.0180 g/cc
0.000650 lb/in³
Minimum
SYNTHOS Koplen® 0513 F Expandable Polystyrene
Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into moldings and smaller blocks.Specific Characteristics: Flammability acc..
Bulk Density 0.0180 - 0.0400 g/cc
0.000650 - 0.00145 lb/in³
Typical
SYNTHOS Koplen® 0513 F Expandable Polystyrene
Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into moldings and smaller blocks.Specific Characteristics: Flammability acc..
Bulk Density >= 0.0180 g/cc
>= 0.000650 lb/in³
Typical
SYNTHOS Koplen® 0513 FR Expandable Polystyrene
Low Pentane Self-Extinguishing type Koplen®.Processing Method: Expansion of beads by water steam, hot water or hot air. Shaping into products and smaller blocks. Lower density can be achieved aft..
Bulk Density 0.0180 g/cc
0.000650 lb/in³
Minimum
SYNTHOS Koplen® 2040 F Expandable Polystyrene
Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into blocks.Specific Characteristics: Flammability according to CSN EN ISO ..
Bulk Density 0.0180 - 0.0350 g/cc
0.000650 - 0.00126 lb/in³
BASF Styropor® KF 462M EPS
Description: Expandable polystyrene (EPS) with pentane as a blowing agent. For the production of expanded foam. Block having bulk densities of 18-35 kg/m3 and fire characteristics in conformity with..