Polymer Property : Bulk Density = 0.000578 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.0160 g/cc
0.000578 lb/in³
Minimum
SYNTHOS Koplen® 0814 F Expandable Polystyrene
Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to moldings and block.Specific Characteristics: Flammability ..
Bulk Density 0.0160 - 0.0400 g/cc
0.000578 - 0.00145 lb/in³
Typical
SYNTHOS Koplen® 0814 F Expandable Polystyrene
Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to moldings and block.Specific Characteristics: Flammability ..
Bulk Density >= 0.0160 g/cc
>= 0.000578 lb/in³
Typical
SYNTHOS Koplen® 0814 FR Expandable Polystyrene
Low Pentane Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to molded bricks and blocks. Lower density can be..
Bulk Density 0.0160 - 0.0350 g/cc
0.000578 - 0.00126 lb/in³
BASF E-por® 0.02 g/cc Density; Styrene and Ethylene (Europe)
Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e..
Bulk Density 0.0160 - 0.0350 g/cc
0.000578 - 0.00126 lb/in³
BASF E-por® 0.025 g/cc Density; Styrene and Ethylene (Europe)
Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e..
Bulk Density 0.0160 - 0.0350 g/cc
0.000578 - 0.00126 lb/in³
BASF E-por® 0.035 g/cc Density; Styrene and Ethylene (Europe)
Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e..
Bulk Density 0.0160 - 0.0300 g/cc
0.000578 - 0.00108 lb/in³
BASF Styropor® KF 362M EPS
Description: Expandable polystyrene (EPS) with pentane as a blowing agent. For the production of expanded foam. Block having bulk densities of 16-30 kg/m3 and fire characteristics in conformity with..
Bulk Density 0.0160 - 0.0350 g/cc
0.000578 - 0.00126 lb/in³
BASF E-por® 0.03 g/cc Density; Styrene and Ethylene (Europe)
Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e..
Copyright © lookpolymers.com All Rights Reserved