Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.0150 - 0.0300 g/cc | 0.000542 - 0.00108 lb/in³ | Typical |
SYNTHOS Koplen® 1640 F Expandable Polystyrene Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into blocks.Specific Characteristics: Flammability according to CSN EN ISO .. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 A 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 A 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 D 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 D 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 D 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 K 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 K 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |
|||
Bulk Density | 0.0120 - 0.0300 g/cc | 0.000434 - 0.00108 lb/in³ | |
BASF Styropor® KF 162M EPS Description: Expandable polystyrene (EPS) with pentane as a blowing agent. For the production of expanded foam. Block having bulk densities of 12-30 kg/m3 and fire characteristics in conformity with.. |
|||
Bulk Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | |
BASF Styropor® KF 362M EPS Description: Expandable polystyrene (EPS) with pentane as a blowing agent. For the production of expanded foam. Block having bulk densities of 16-30 kg/m3 and fire characteristics in conformity with.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 A 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Bulk Density | 0.0120 - 0.0300 g/cc | 0.000434 - 0.00108 lb/in³ | |
BASF Styropor® KF 262M EPS Description: Expandable polystyrene (EPS) with pentane as a blowing agent. For the production of expanded foam. Block having bulk densities of 12-30 kg/m3 and fire characteristics in conformity with.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 A 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 D 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 K 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 K 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |