Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 A 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 A 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 D 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 D 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 D 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 K 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 K 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 A 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 A 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 D 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 K 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |
|||
Bulk Density | 0.0260 - 0.0300 g/cc | 0.000939 - 0.00108 lb/in³ | |
BASF Neopolen® P 9230 K 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |