Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Typical |
SYNTHOS Koplen® 0822 FR Expandable Polystyrene Low Pentane Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to molded bricks and blocks. Lower density can be.. |
|||
Bulk Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Typical |
SYNTHOS Koplen® 1020 FR Expandable Polystyrene Low Pentane Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into thick walled products and blocks. Lower density can be ach.. |
|||
Bulk Density | 0.0120 - 0.0300 g/cc | 0.000434 - 0.00108 lb/in³ | |
BASF Styropor® KF 162M EPS Description: Expandable polystyrene (EPS) with pentane as a blowing agent. For the production of expanded foam. Block having bulk densities of 12-30 kg/m3 and fire characteristics in conformity with.. |
|||
Bulk Density | 0.0120 - 0.0300 g/cc | 0.000434 - 0.00108 lb/in³ | |
BASF Styropor® KF 262M EPS Description: Expandable polystyrene (EPS) with pentane as a blowing agent. For the production of expanded foam. Block having bulk densities of 12-30 kg/m3 and fire characteristics in conformity with.. |