Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion Beryllium Copper Alloy 165 Forgings & Extrusions; A (TB00) Temper (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion Beryllium Copper Alloy 165 Forgings & Extrusions; AT (TF00) Temper (UNS C17000) Treatment required for max strength: 3 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; AT (TF00) Temper; All Thicknesses (UNS C17000) Treatment required for max strength: 3 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; H (TD04) Temper; over 51 to 76 mm Thickness (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; H (TD04) Temper; over 9.5 to 25 mm Thickness (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; H (TD04) Temper; up to 9.5 mm Thickness (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; HT (TH04) Temper; over 25 to 51 mm Thickness (UNS C17000) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; HT (TH04) Temper; over 51 to 76 mm Thickness (UNS C17000) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; HT (TH04) Temper; over 9.5 to 25 mm Thickness (UNS C17000) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion Beryllium Copper Alloy 165 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion Beryllium Copper Alloy 165 Rod and Bar; AT (TF00) Temper; over 76 mm (UNS C17000) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion Beryllium Copper Alloy 165 Rod and Bar; AT (TF00) Temper; up to 76 mm (UNS C17000) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion Beryllium Copper Alloy 165 Rod and Bar; H (TD04) Temper; over 9.5 to 25.4 mm (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion Beryllium Copper Alloy 165 Rod and Bar; H (TD04) Temper; up to 9.5 mm (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion Beryllium Copper Alloy 165 Rod and Bar; HT (TH04) Temper; over 25.4 to 76 mm (UNS C17000) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion Beryllium Copper Alloy 165 Rod and Bar; HT (TH04) Temper; over 9.5 to 25.4 mm (UNS C17000) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion Beryllium Copper Alloy 165 Rod and Bar; HT (TH04) Temper; up to 9.5 mm (UNS C17000) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion BrushCAST® 165C High Strength Casting Alloy (As Cast & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion BrushCAST® 165C High Strength Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion BrushCAST® 165CT Fine Grain Casting Alloy (As Cast & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion BrushCAST® 165CT Fine Grain Casting Alloy (As Cast) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Indium Corp. Indalloy® Sn62 Sn-Pb-Ag Solder Alloy Good general purpose solder. Can be used on silver bearing surfaces to reduce scavenging.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Materion BrushCAST® 165C High Strength Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Indium Corp. Indalloy 104 Tin-Lead Solder Alloy Widely used electronic solder. Good for silver metallization. Has improved strength and fatigue propertiesInformation Provided by Indium Corporation |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Williams Advanced Alloys WS179 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
Chicago Extruded Metals BioBrass® UNS C46400 Copper-Zinc-Tin Alloy Copper-Zinc-Tin Alloy (Naval Brass)Finished product available as bar, wire, rod, forged, or shapes.Chicago Extruded Metal temper codes: H01, H02, H04, M30Information provided by Chicago Extruded Met.. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
California Fine Wire Stablohm 650 Nickel Chromium Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
ATI Allvac® 35N Nickel Superalloy, Heat Treatment: 1052°C (1925°F) + Age Data provided by Allvac.Applications: Aircraft fasteners. Line wire for down-hole instrumentation. Biomedical devices, high fatigue strength applications. |
|||
Density | 8.41 g/cc | 0.304 lb/in³ | |
ATI Allvac® Nickelvac® 600 Nickel Superalloy, Heat Treatment: 927°C (1700°F) Anneal Data provided by Allvac.Applications: Aircraft engines, nuclear reactor applications, chemical process equipment, high temperature fixtures. |