Material Notes:
Data provided by Allvac.Applications: Aircraft fasteners. Line wire for down-hole instrumentation. Biomedical devices, high fatigue strength applications.
Physical Properties Metric English Comments
Density 8.41 g/cc
0.304 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 278
278
Estimated from Rockwell C value for Brinell test with 3000 kg load/10 mm diameter ball
Hardness, Knoop 301
301
Estimated from Rockwell C value.
Hardness, Rockwell C 28
28
Hardness, Vickers 292
292
Estimated from Rockwell C value.
Tensile Strength, Ultimate 897 MPa
130000 psi
Tensile Strength, Yield 517 MPa

@Strain 0.200 %
75000 psi

@Strain 0.200 %
Elongation at Break 30 %
30 %
Reduction of Area 35 %
35 %
Component Elements Properties Metric English Comments
Carbon, C 0.013 %
0.013 %
Chromium, Cr 20 %
20 %
Cobalt, Co 35 %
35 %
as balance
Molybdenum, Mo 9.8 %
9.8 %
Nickel, Ni 35 %
35 %