Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. Indalloy® Sn62 Sn-Pb-Ag Solder Alloy

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy , Tin Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® Sn62 Sn-Pb-Ag Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good general purpose solder. Can be used on silver bearing surfaces to reduce scavenging.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 8.41 g/cc
0.304 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 48.3 MPa
7010 psi
Shear Strength 52.0 MPa
7540 psi
Shear Bond Holding Strength
Thermal Properties Metric English Comments
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 50.0 W/m-K

@Temperature 85.0 °C
347 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 179 - 179 °C
354 - 354 °F
Solidus 179 °C
354 °F
Liquidus 179 °C
354 °F
Component Elements Properties Metric English Comments
Lead, Pb 36 %
36 %
Silver, Ag 2.0 %
2.0 %
Tin, Sn 62 %
62 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000140 ohm-cm
0.0000140 ohm-cm
Users viewing this material also viewed the following: