Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.65 g/cc | 0.276 lb/in³ | Coating Property |
The NanoSteel® Company SHS 7574 HVOF Steel Alloy, Atomized Powder Coating Description: SHS 7574 HVOF is an iron based steel alloy with a nanoscale microstructure that features extreme corrosion resistance in high chlorine, salt fog, concentrated salt and seawater .. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
CeramTec Sonox® P5 Piezoceramic Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics .. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
CeramTec Sonox® P504 Piezoceramic Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics .. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
American Elements C-MITE™ Cerium Oxide Nanopowder General DescriptionApplicationsC-MITE™ powders and dispersions recently developed are inorganic cerium-oxide nanoparticles with unique polishing and Ultra-Violet attenuating properties. C-MITE-A™ .. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition RH 950 AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel 18 Cr-Cb™ Ferritic Stainless steel AK Steel 18 Cr-Cb™ provides a more effective solution than Type 409 to many automotive exhaust applications, due to its higher oxidation resistance, improved creep resistance and moderate formabili.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel CARLITE® M-3 Grain Oriented Electrical Steel Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel CARLITE® M-6 Grain Oriented Electrical Steel Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel DI-MAX® M-15 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel TRAN-COR® H-0 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel TRAN-COR® H-1 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel TRAN-COR® H-1 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel TRAN-COR® H-2 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ArcelorMittal Torque 20-15 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ArcelorMittal Torque 25-16 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ArcelorMittal Torque 30-17 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition TH 1050 AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel CARLITE® M-5 Grain Oriented Electrical Steel Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | ASTM A34 |
AK Steel DI-MAX® HF-10 Nonoriented Electrical Steel DI-MAX HF-10 is a fully processed nonoriented electrical steel designed for use in high speed motors, traction motors, aircraft generators, and other rotating equipment operating at frequencies abov.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel TRAN-COR® H-0 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 649°C (1200°F) Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
CeramTec Sonox® P4 Piezoceramic Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics .. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Annealed Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 204°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 288°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 316°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 427°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 482°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 538°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410HC Allegheny Ludlum Type 410HC is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainl.. |