Material Notes:
Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics require very little energy and their shape potential is almost unlimited. Such properties allow this material to be used in wide-ranging apparatus and mechanical engineering applications. Sonox® P504 is designed specifically for sensors.
Physical Properties Metric English Comments
Density 7.65 g/cc
0.276 lb/in³
Electrical Properties Metric English Comments
Curie Temperature 350 °C
662 °F
Tc
Dielectric Constant 835
835
e33 S/e?
1085
1085
e11 S/e?
1730
1730
e33 T/e?
1920
1920
e11 T/e?
Dissipation Factor 0.012
0.012
tand
Piezoelectric Longitudinal Coupling Factor, k33 0.71
0.71
Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V -157
-157
Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V 530
530
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 25.5
25.5
Piezoelectric Planar Coupling Factor, kp 0.59
0.59
Piezoelectric Mechanical Q 90
90
Piezoelectric Shear Coupling Factor, k15 0.66
0.66
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 390
390
Piezoelectric Transverse Coupling Factor, k31 0.32
0.32
Descriptive Properties Value Comments
Aging Rates (%/decade) 0.1
Ck
0.4
Cf
-0.4
Ce
Elastic Compliance (10^-12 m²/N) 16.3
s11^E
17.5
s33^E
Elastic Rigidity (10^10 N/m²) 14.9
c33^D
4.4
c55^D
Frequency Constants (kHz·mm) 1250
N3
1320
N1
2020
Np
2035
Nt
Piezoelectric Coupling Coefficient, kt 0.51