Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.63 g/cc | 0.276 lb/in³ | |
Indium Corp. Indalloy 13 Indium Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
Schmolz + Bickenbach 416RS Stainless Steel Bar Description: Ugitech’s 416RS is a low sulfur pre-hardened chrome bearing martensitic stainless steel specifically designed for the precision rifle barrel industry. The 416RS chemistry is balanc.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
CeramTec Sonox® P5 Piezoceramic Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics .. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
Crucible Steel 440C Chromium Steel Crucible 440C is a hardenable chromium steel. It has one of the highest attainable hardnesses of the corrosion and heat resisting grades. This grade is magnetic at all times.Information provided b.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
Crucible Steel CSM® 420 XL Stainless Steel CSM 420 XL is the workhorse premium quality stainless mold steel designed for applications requiring a combination of corrosion resistance and wear resistance. It is double melted for the microstruc.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel CARLITE® M-4 Grain Oriented Electrical Steel Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel DI-MAX® M-15 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel TRAN-COR® H-1 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel TRAN-COR® H-1 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel TRAN-COR® H-2 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Density | 7.64 g/cc @Temperature 200 °C |
0.276 lb/in³ @Temperature 392 °F |
|
Assab Steels ASSAB XW-41 Cold Work Steel XW-41 is a high-carbon, high chromium tool steel alloyed with molybdenum and vanadium characterized by:High wear resistanceHigh compressive strength Good through-hardening propertiesHigh stability i.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum 410 Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum AL 403™ Martensitic Stainless Steel Characteristics: corrosion resistant, heat resistant, oxidation resistant up to 1400°F.Information provided by Allegheny Ludlum |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 649°C (1200°F) (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ArcelorMittal Torque 25-16 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ArcelorMittal Torque 27-16 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ArcelorMittal Torque 30-18 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition TH 1050 AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel CARLITE® M-5 Grain Oriented Electrical Steel Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
AK Steel TRAN-COR® H-0 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 760°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 704°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
CeramTec Sonox® P4 Piezoceramic Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics .. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Annealed Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 316°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 427°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 538°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.65 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410HC Allegheny Ludlum Type 410HC is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainl.. |