Material Notes:
Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics require very little energy and their shape potential is almost unlimited. Such properties allow this material to be used in wide-ranging apparatus and mechanical engineering applications. Sonox® P5 is a highly sensitive material characterized by dielectric constants in the 1000 to 4000 range and low Q factors that are < 100. It is used in a wide range of sensor applications, as well as for actuators. P5 is specifically used for sensor technology, materials testing, and medical diagnostics and treatment. It is also used to make impact type igniters.
Physical Properties Metric English Comments
Density 7.65 g/cc
0.276 lb/in³
Electrical Properties Metric English Comments
Curie Temperature 340 °C
644 °F
Tc
Dielectric Constant 865
865
e33 S/e?
1220
1220
e11 S/e?
1850
1850
e11 T/e?
1850
1850
e33 T/e?
Dissipation Factor 0.020
0.020
tand
Piezoelectric Longitudinal Coupling Factor, k33 0.73
0.73
Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V -180
-180
Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V 550
550
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 27.5
27.5
Piezoelectric Planar Coupling Factor, kp 0.62
0.62
Piezoelectric Mechanical Q 90
90
Piezoelectric Shear Coupling Factor, k15 0.72
0.72
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 450
450
Piezoelectric Transverse Coupling Factor, k31 0.34
0.34
Descriptive Properties Value Comments
Aging Rates (%/decade) 0.1
Ck
0.3
Cf
-2.3
Ce
Capacitance (pF) 30
CT-Type 39604
32
CT-Type 39610
39
CT-Type 39606
Elastic Compliance (10^-12 m²/N) 17.1
s11^E
19
s33^E
Elastic Rigidity (10^10 N/m²) 14.5
c33^D
5.8
c55^D
Frequency Constants (kHz·mm) 1310
N3
1380
N1
1900
Nt
2030
Np
Piezoelectric Coupling Coefficient, kt 0.49
Piezoelectric Voltage Coefficient, e33 (C/m²) 16.3