Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 6.50 g/cc | 0.235 lb/in³ | |
MarkeTech Thorium-Doped Lanthanum Aluminum Oxide (Th:LaAlO3) Single Crystal Substrate Data provided by MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors. |
|||
Density | 6.50 g/cc | 0.235 lb/in³ | |
Indium Corp. Indalloy® 51 Ga-In-Sn Alloy for Mercury Replacement Alloy liquid at room temperature, wets glass and quartz. Mercury replacement.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 6.50 g/cc | 0.235 lb/in³ | |
Indium Corp. Indalloy® 46L Ga-In-Sn-Zn Alloy for Mercury Replacement Alloy liquid at room temperature, wets glass and quartz. Mercury replacement.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 6.50 g/cc | 0.235 lb/in³ | |
Special Metals Nitinol Body-Temperature Ni-Ti alloy Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology. |
|||
Density | 6.50 g/cc | 0.235 lb/in³ | |
Special Metals Nitinol Chrome-Doped Superelastic Ni-Ti alloy Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology. |
|||
Density | 6.50 g/cc | 0.235 lb/in³ | |
Special Metals Nitinol High-Strength Superelastic Ni-Ti alloy Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology. |
|||
Density | 6.50 g/cc | 0.235 lb/in³ | |
Special Metals Nitinol High-Strength Superelastic Ni-Ti-Fe alloy Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology. |
|||
Density | 6.50 g/cc | 0.235 lb/in³ | |
Special Metals Nitinol High-Temperature Shape Memory Ni-Ti alloy Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology. |
|||
Density | 6.50 g/cc | 0.235 lb/in³ | |
Special Metals Nitinol High-Temperature Shape Memory Ni-Ti alloy Ribbon Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology. |
|||
Density | 6.50 g/cc | 0.235 lb/in³ | |
Special Metals Nitinol Superelastic Ni-Ti alloy Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology. |
|||
Density | 6.50 g/cc | 0.235 lb/in³ | |
Goodfellow Nickel 55/Titanium 45 Shape Memory Alloy Shape memory alloy is a description applied to that group of metallic materials which show the ability to return to the previously defined shape or size when subjected to the correct thermal procedu.. |
|||
Density | 6.50 g/cc | 0.235 lb/in³ | |
American Elements Lanthanum Oxide Nanopowder General DescriptionLanthanum Oxide (LaO) Nanoparticles, nanodots or Nanopowder are white spherical high surface area metal particles. Nanoscale Lanthanum Oxide Particles are typically 10-30 nanomete.. |
|||
Density | 6.50 g/cc | 0.235 lb/in³ | |
China Tungsten NT4 Titanium Carbonitride Alloy Titanium carbonitride base alloy , also called cermets, with of high hardness, good red hard-ness and wear resistance, medium toughness, high corrosion resistance to acids and alkalis and hi-tempe.. |
|||
Density | >= 6.50 g/cc | >= 0.235 lb/in³ | |
China Tungsten STG60-20 PM Structural Parts Information provided by China Tungsten |
|||
Density | >= 6.50 g/cc | >= 0.235 lb/in³ | |
China Tungsten STG60Cu3Mo40 PM Structural Parts Information provided by China Tungsten |
|||
Density | >= 6.50 g/cc | >= 0.235 lb/in³ | |
China Tungsten STG70Cu-35 PM Structural Parts Information provided by China Tungsten |
|||
Density | >= 6.50 g/cc | >= 0.235 lb/in³ | |
China Tungsten STG90-25 PM Structural Parts Information provided by China Tungsten |
|||
Density | >= 6.50 g/cc | >= 0.235 lb/in³ | |
China Tungsten STG30-15 PM Structural Parts Information provided by China Tungsten |
|||
Density | 6.50 g/cc | 0.235 lb/in³ | |
ATI Wah Chang Zircadyne® Alloy Zr 702 Zircadyne 702 is commercially pure zirconium. Alloy exhibits good ductility even at cryogenic temperatures and good strength comparable with other common engineering alloys.Information provided by A.. |