Material Notes:
Information provided by China Tungsten
Physical Properties Metric English Comments
Density >= 6.50 g/cc
>= 0.235 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell <= 120
<= 120
Elongation at Break >= 0.50 %
>= 0.50 %
Component Elements Properties Metric English Comments
Carbon, C 0.40 - 0.70 %
0.40 - 0.70 %
Copper, Cu 2.0 - 4.0 %
2.0 - 4.0 %
Iron, Fe 92.8 - 95.6 %
92.8 - 95.6 %
Molybdenum, Mo 0.50 - 1.0 %
0.50 - 1.0 %
Other 1.5 %
1.5 %
Descriptive Properties Value Comments
Impact Ductility (MPa), min 0.05