American Elements Lanthanum Oxide Nanopowder

Category Ceramic , Oxide
Manufacturer American Elements
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements Lanthanum Oxide Nanopowder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionLanthanum Oxide (LaO) Nanoparticles, nanodots or Nanopowder are white spherical high surface area metal particles. Nanoscale Lanthanum Oxide Particles are typically 10-30 nanometers (nm) with specific surface area (SSA) in the 130-150 m 2 /g range. Nano Lanthanum Oxide Particles are also available in passivated and in Ultra high purity and high purity and carbon coated and dispersed forms. Applications for Lanthanum Oxide nanocrystals include in preparation of various perovskite nanostructures (such as lanthanum manganite and lanthanum chromite) for the cathode layer of solid oxide fuel cells (SOFC), as a Magnetic Nanoparticle (also as iron oxide -lanthanum oxide nanoparticles) for magnetic data storage and magnetic resonance imaging (MRI), in biosensors, for phosphate removal in bio medical and water treatment (including swimming pools and spas) applications, in laser crystals and optics, and in nanowire, nanofiber and in certain alloy and catalyst applications. Further research is being done for their potential electrical, dielectric, magnetic, optical, imaging, catalytic, biomedical and bioscience uses.
Physical Properties Metric English Comments
Density 6.50 g/cc
0.235 lb/in³
Particle Size 0.010 - 0.030 µm
0.010 - 0.030 µm
Specific Surface Area 130 - 150 m²/g
130 - 150 m²/g
Molecular Weight 325.82 g/mol
325.82 g/mol
Thermal Properties Metric English Comments
Melting Point 2305 °C
4181 °F
Boiling Point 4200 °C
7590 °F
Descriptive Properties Value Comments
Appearance White
Solubility Insoluble in water, moderately soluble in strong mineral acids
Stability Strongly hygroscopic