Shape memory alloy is a description applied to that group of metallic materials which show the ability to return to the previously defined shape or size when subjected to the correct thermal procedure. Uses include blood clot filters, cryogenic coupling rings, proportional control valves and orthodontic correction.Information provided by Goodfellow.
Physical Properties Metric English Comments
Density 6.50 g/cc
0.235 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 1140 MPa
165000 psi
Elongation at Break 15 - 40 %
15 - 40 %
Tensile Modulus 60.0 - 90.0 GPa
8700 - 13100 ksi
Thermal Properties Metric English Comments
CTE, linear 6.60 µm/m-°C

@Temperature 20.0 °C
3.67 µin/in-°F

@Temperature 68.0 °F
Martensitic
11.0 µm/m-°C

@Temperature 20.0 °C
6.11 µin/in-°F

@Temperature 68.0 °F
Austenitic
Thermal Conductivity 8.60 W/m-K
59.7 BTU-in/hr-ft²-°F
Martensitic
18.0 W/m-K
125 BTU-in/hr-ft²-°F
Austenitic
Melting Point 1310 °C
2390 °F
Component Elements Properties Metric English Comments
Nickel, Ni 55 %
55 %
Titanium, Ti 45 %
45 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000100 ohm-cm
0.0000100 ohm-cm
Austenitic
0.0000800 ohm-cm
0.0000800 ohm-cm
Martensitic